HelpContactFor teachers and institutes
>_StemPy Lab
Mock TestsClasses

>_StemPy Lab

Learn. Solve. Code the solutions. Test yourself.

Live examsFree mock exams, timed and rankedEveryone starts together, and your score and rank come the moment it ends.See the exams →
Live examsInternational live exams are comingTell us which exam you want first. Timed practice papers are open now.See what is coming →

Learn

  • Physics
  • Chemistry
  • Mathematics
  • Biology
  • Python Programming
  • Statistics & Data Science
  • Computer Science
  • Space Science and Astronomy
  • Classes
  • Groups

Practice

  • Problems
  • Quizzes
  • Mock Tests
  • Prepare for an Exam
  • Question Sets
  • Exams
  • Certificates
  • Python Labs
  • AI Practice Generator
  • Student-Created Tests

Community

  • Discussions
  • Resources
  • Notes
  • Glossary
  • Blog

Account

  • Log in
© 2026 senLearn. All rights reserved.HelpFor SchoolsAboutContactPrivacy PolicyTerms of UseRefund Policy
Ores and Their Concentration: Minerals, Flotation, Leaching and Roasting
  1. 1Minerals, ores and gangue: where metals come from
  2. 2Concentrating an ore: washing, magnets, froth and leaching
  3. 3Calcination, roasting, flux and slag
  1. Chemistry
  2. /Ores and Their Concentration: Minerals, Flotation, Leaching and Roasting
  3. /Concentrating an ore: washing, magnets, froth and leaching

Course 35.1·Lesson 2 of 3

Concentrating an ore: washing, magnets, froth and leaching

A ton of copper ore may hold only a few kilograms of copper. Before anything is heated, the gangue must go. This lesson explains four ways to concentrate an ore: hydraulic washing, magnetic separation, froth flotation and leaching, with the Bayer and cyanide processes.

about 25 min1 simulation1 practice question
Lesson 2 of 3Show all lessonsHide
Ores and Their Concentration: Minerals, Flotation, Leaching and Roasting
  1. 1Minerals, ores and gangue: where metals come from
  2. 2Concentrating an ore: washing, magnets, froth and leaching
  3. 3

Try the code and the simulations beside the lesson.

Why concentrate first?

Heating a whole mountain of rock to get a little metal wastes fuel and furnace space. So we first remove most of the gangue. The method depends on a difference between the mineral and the gangue: density, magnetism, how the surface takes up oil, or how the mineral dissolves. Concentration is also called dressing or benefaction of the ore.

Hydraulic washing

This is gravity separation. Powdered ore is washed by an upward stream of running water. The lighter gangue is carried away, and the heavier mineral stays behind. It works when the ore is much denser than the gangue, as for the oxide ores of tin and for gold in sand.

Magnetic separation

If either the mineral or the gangue is attracted by a magnet, a magnetic roller separates them. Magnetite, chromite and pyrolusite are attracted. Tin stone (cassiterite, SnO2\text{SnO}_{2}SnO2​) is not magnetic, but the wolframite mixed with it is, so the magnet removes the wolframite.

Magnetic separation. Powdered ore falls from a hopper onto a belt that runs over two rollers. The right roller is a magnet. The non-magnetic gangue flies off the end of the belt and lands in a near heap. The magnetic particles stick to the belt a little longer and drop in a second heap, under the roller, labelled magnetic mineral.

Froth flotation

This method is used mainly for sulphide ores. The powdered ore is mixed with water to a thin mud called the pulp. Two kinds of reagent are added.

  • Collectors, such as pine oil, fatty acids and xanthates, make the surface of the sulphide water-repellent. The mineral then sticks to air bubbles.
  • Froth stabilisers, such as cresols and aniline, keep the froth from breaking.

A stirrer beats air into the pulp. The bubbles carry the sulphide particles to the top, where a froth forms and is skimmed off. The gangue is wetted by the water and sinks.

A froth flotation cell drawn in section. A tank holds a grey pulp of powdered ore, water and oil. A stirrer in the middle beats air in through a pipe at the bottom, and air bubbles rise. Dark sulphide particles stick to the bubbles and collect in a froth on top, which flows over the lip into a launder labelled froth with the mineral. Pale gangue particles sink and leave at the bottom, labelled gangue with water.

Depressants let us separate two sulphides. For an ore of galena, PbS\text{PbS}PbS, with zinc blende, ZnS\text{ZnS}ZnS, sodium cyanide is added. It forms a zinc cyanide complex on the surface of the zinc blende, so the zinc blende does not float. Galena comes up with the froth first. Later the zinc blende can be activated and floated.

A flotation balance. Plants judge flotation by two numbers. Let fff, ccc and ttt be the percentages of metal in the feed, the concentrate and the tailings (the rejected part). Mass and metal are both conserved. From these two balances,

mass of concentrate=feed×f−tc−t\displaystyle \text{mass of concentrate} = \text{feed} \times \dfrac{f - t}{c - t}mass of concentrate=feed×c−tf−t​
R=c (f−t)f (c−t)\displaystyle R = \dfrac{c\,(f - t)}{f\,(c - t)}R=f(c−t)c(f−t)​

where RRR is the recovery, the share of the metal that reaches the concentrate.

Set f=1.5 %f = 1.5\ \%f=1.5 %, c=24 %c = 24\ \%c=24 % and move ttt. Each extra 0.05 % of copper left in the tailings costs a few percent of the recovery, because the tailings are almost all of the mass.

Leaching

In leaching the mineral dissolves in a suitable reagent and the gangue does not.

The Bayer process for bauxite. Bauxite holds silica, iron oxides and titanium oxide as impurities. It is digested with a concentrated solution of sodium hydroxide at 473 to 523 K under pressure. Alumina dissolves as sodium aluminate. Iron oxide does not dissolve, and it is filtered off as a red mud.

Al2O3(s) + 2NaOH(aq) + 3H2O(l) → 2Na[Al(OH)4](aq)\text{Al}_{2}\text{O}_{3}(\text{s})\ +\ 2\text{NaOH}(\text{aq})\ +\ 3\text{H}_{2}\text{O}(\text{l})\ \rightarrow \ 2\text{Na}[\text{Al}(\text{OH})_{4}](\text{aq})Al2​O3​(s) + 2NaOH(aq) + 3H2​O(l) → 2Na[Al(OH)4​](aq)

The solution is then neutralised by passing in carbon dioxide, and seeded with a little freshly prepared hydrated alumina. Hydrated alumina comes out.

2Na[Al(OH)4](aq) + CO2(g) → Al2O3⋅xH2O(s) + 2NaHCO3(aq)2\text{Na}[\text{Al}(\text{OH})_{4}](\text{aq})\ +\ \text{CO}_{2}(\text{g})\ \rightarrow \ \text{Al}_{2}\text{O}_{3}\cdot \text{xH}_{2}\text{O}(\text{s})\ +\ 2\text{NaHCO}_{3}(\text{aq})2Na[Al(OH)4​](aq) + CO2​(g) → Al2​O3​⋅xH2​O(s) + 2NaHCO3​(aq)

Silica stays in the solution as sodium silicate. The hydrated alumina is filtered, dried and heated to about 1470 K to give pure alumina.

Al2O3⋅xH2O(s) → Al2O3(s) + xH2O(g)\text{Al}_{2}\text{O}_{3}\cdot \text{xH}_{2}\text{O}(\text{s})\ \rightarrow \ \text{Al}_{2}\text{O}_{3}(\text{s})\ +\ \text{xH}_{2}\text{O}(\text{g})Al2​O3​⋅xH2​O(s) → Al2​O3​(s) + xH2​O(g)

The cyanide process for gold and silver. The ore is leached with dilute sodium cyanide solution in the presence of air. Oxygen oxidises the metal, and cyanide holds it in solution as a complex.

4M(s) + 8CN−(aq) + 2H2O(l) + O2(g) → 4[M(CN)2]−(aq) + 4OH−(aq)4\text{M}(\text{s})\ +\ 8\text{CN}^{-}(\text{aq})\ +\ 2\text{H}_{2}\text{O}(\text{l})\ +\ \text{O}_{2}(\text{g})\ \rightarrow \ 4[\text{M}(\text{CN})_{2}]^{-}(\text{aq})\ +\ 4\text{OH}^{-}(\text{aq})4M(s) + 8CN−(aq) + 2H2​O(l) + O2​(g) → 4[M(CN)2​]−(aq) + 4OH−(aq) with M = Ag or Au

Zinc, a more reactive metal, then displaces the gold or silver.

2[M(CN)2]−(aq) + Zn(s) → [Zn(CN)4]2−(aq) + 2M(s)2[\text{M}(\text{CN})_{2}]^{-}(\text{aq})\ +\ \text{Zn}(\text{s})\ \rightarrow \ [\text{Zn}(\text{CN})_{4}]^{2-}(\text{aq})\ +\ 2\text{M}(\text{s})2[M(CN)2​]−(aq) + Zn(s) → [Zn(CN)4​]2−(aq) + 2M(s)

Low-grade copper ores and copper scrap are leached with acid or with bacteria. The solution of copper(II) ions is then treated with scrap iron or hydrogen, which gives copper. This route is called hydrometallurgy.

Practise with new numbers

Try it in Python

The program works out the mass of concentrate and the recovery of a flotation circuit.

Read it first. Predict the recovery if the tailings held no copper at all. Then run it.

1. Change t to 0.05. How much does the recovery rise?

2. Change c to 30.0 and keep the rest. Does more or less concentrate come out?

Common mistakes

  • Using froth flotation for an oxide ore. It suits sulphides, whose surfaces take up the collector.
  • Mixing up the reagents. Pine oil and xanthates collect. Cresols and aniline stabilise the froth. Sodium cyanide depresses zinc blende.
  • Forgetting the air in the cyanide process. Oxygen is the oxidising agent. Without it the gold does not dissolve.
  • Thinking iron oxide dissolves in the Bayer process. It stays behind as red mud. Silica dissolves.

Remember these

  • Hydraulic washing: density. Magnetic separation: magnetism. Froth flotation: sulphides. Leaching: solubility.
  • Bayer: alumina dissolves in hot sodium hydroxide, carbon dioxide and seeding bring back hydrated alumina, heating at 1470 K gives alumina.
  • Cyanide: gold and silver dissolve as [M(CN)2]−[\text{M}(\text{CN})_{2}]^{-}[M(CN)2​]− in air, and zinc displaces them.

References

  • NCERT Chemistry Part I for Class 12 (2007 edition), Unit 6, the section on the concentration of ores.
  • Greenwood and Earnshaw, Chemistry of the Elements, the chapters on aluminium and on copper, silver and gold.

Check yourself

Try each one on your own first. If you are stuck, open a hint. Then check with Show the answer.

  1. Why is froth flotation used for sulphide ores and not for most oxide ores?
  1. In the Bayer process, what are the roles of the sodium hydroxide and of the carbon dioxide?
  1. A mixture of galena and zinc blende is floated with sodium cyanide added. Which mineral comes up first, and why?
  1. Which substance is oxidised and which is reduced when zinc is added to a solution of [Au(CN)2]−[\text{Au}(\text{CN})_{2}]^{-}[Au(CN)2​]−?

Enroll free in Ores and Their Concentration: Minerals, Flotation, Leaching and Roasting

Every lesson is open to read. Enrolling also lets you:

  • Mark lessons done and carry on where you stopped.
  • Take the tests of this lesson and its course.
  • Count the course towards the certificate for its chapter.
No payment. You can leave at any time.

Problems (3)

A flotation plant treats 1000 tonnes of crushed copper ore each day…Hard · High School (11–12) · by StemPy Lab
A tonne of bauxite holds 55.0 % alumina, Al₂O₃, and 6.0 % silica, SiO₂…Advanced · High School (11–12) · by StemPy Lab
A gold mine leaches 1000 tonnes of ore each day…Hard · High School (11–12) · by StemPy Lab
Next: lesson 3Calcination, roasting, flux and slag
← Ores and Their Concentration: Minerals, Flotation, Leaching and Roasting
← Minerals, ores and gangue: where metals come fromCalcination, roasting, flux and slag →

Discussion (0)

Log in to join the discussion.

Loading…

1 Python program
4 questions to check yourself

This lesson is free to read. Enroll free to keep your place and take the tests.

Calcination, roasting, flux and slag

Python Labs (1)

A flotation balancePython Lab · by StemPy Lab