  • Physics
  • Chemistry
  • Mathematics
  • Biology
  • Python Programming
  • Statistics & Data Science
  • Computer Science
  • Space Science and Astronomy
  • Classes
  • Groups

Practice

  • Problems
  • Quizzes
  • Mock Tests
  • Prepare for an Exam
  • Question Sets
  • Exams
  • Certificates
  • Python Labs
  • AI Practice Generator
  • Student-Created Tests

Community

  • Discussions
  • Resources
  • Notes
  • Glossary
  • Blog

Account

  • Log in
© 2026 senLearn. All rights reserved.HelpFor SchoolsAboutContactPrivacy PolicyTerms of UseRefund Policy
Ores and Their Concentration: Minerals, Flotation, Leaching and Roasting
  1. 1Minerals, ores and gangue: where metals come from
  2. 2Concentrating an ore: washing, magnets, froth and leaching
  3. 3Calcination, roasting, flux and slag
  1. Chemistry
  2. /Ores and Their Concentration: Minerals, Flotation, Leaching and Roasting
  3. /Calcination, roasting, flux and slag

Course 35.1·Lesson 3 of 3

Calcination, roasting, flux and slag

Before an ore is reduced it is heated, either alone or in air. Which ores are calcined and which are roasted? This lesson explains calcination and roasting with their equations, the use of a flux to turn gangue into slag, and the self-reduction of galena.

about 25 min1 simulation1 practice question
Lesson 3 of 3Show all lessonsHide
Ores and Their Concentration: Minerals, Flotation, Leaching and Roasting
  1. 1Minerals, ores and gangue: where metals come from
  2. 2Concentrating an ore: washing, magnets, froth and leaching
  3. 3

Try the code and the simulations beside the lesson.

Calcination

Calcination is heating an ore strongly in a limited supply of air, or with none, below its melting point. Water and carbon dioxide are driven off, and volatile impurities leave. It suits carbonates and hydrated oxides.

Fe2O3⋅xH2O(s) → Fe2O3(s) + xH2O(g)\text{Fe}_{2}\text{O}_{3}\cdot \text{xH}_{2}\text{O}(\text{s})\ \rightarrow \ \text{Fe}_{2}\text{O}_{3}(\text{s})\ +\ \text{xH}_{2}\text{O}(\text{g})Fe2​O3​⋅xH2​O(s) → Fe2​O3​(s) + xH2​O(g)

ZnCO3(s) → ZnO(s) + CO2(g)\text{ZnCO}_{3}(\text{s})\ \rightarrow \ \text{ZnO}(\text{s})\ +\ \text{CO}_{2}(\text{g})ZnCO3​(s) → ZnO(s) + CO2​(g)

CaCO3⋅MgCO3(s) → CaO(s) + MgO(s) + 2CO2(g)\text{CaCO}_{3}\cdot \text{MgCO}_{3}(\text{s})\ \rightarrow \ \text{CaO}(\text{s})\ +\ \text{MgO}(\text{s})\ +\ 2\text{CO}_{2}(\text{g})CaCO3​⋅MgCO3​(s) → CaO(s) + MgO(s) + 2CO2​(g)

The solid also becomes porous, which helps the next step.

Roasting

Roasting is heating an ore in a regular supply of air, below its melting point. It suits sulphides, which are oxidised to oxides. Sulphur dioxide comes off.

2ZnS + 3O2 → 2ZnO + 2SO22\text{ZnS}\ +\ 3\text{O}_{2}\ \rightarrow \ 2\text{ZnO}\ +\ 2\text{SO}_{2}2ZnS + 3O2​ → 2ZnO + 2SO2​

2PbS + 3O2 → 2PbO + 2SO22\text{PbS}\ +\ 3\text{O}_{2}\ \rightarrow \ 2\text{PbO}\ +\ 2\text{SO}_{2}2PbS + 3O2​ → 2PbO + 2SO2​

2Cu2S + 3O2 → 2Cu2O + 2SO22\text{Cu}_{2}\text{S}\ +\ 3\text{O}_{2}\ \rightarrow \ 2\text{Cu}_{2}\text{O}\ +\ 2\text{SO}_{2}2Cu2​S + 3O2​ → 2Cu2​O + 2SO2​

Roasting is done in a reverberatory furnace, in which the hot gases are reflected from the roof onto the ore. Arsenic and antimony come off as volatile oxides. The sulphur dioxide is not let into the air. It is used to make sulphuric acid by the contact process, one mole of acid for each mole of sulphur dioxide.

Set 500 kg and try each sulphide. Zinc blende gives the most sulphur dioxide for a kilogram, because its molar mass is the smallest. Galena gives the least.

Flux and slag

Even a concentrated ore holds some gangue. In the furnace a flux is added. It combines with the gangue to form a slag, a fusible compound that melts and floats on the molten metal, so it can be run off.

  • Acidic gangue needs a basic flux. Silica in an iron ore is removed with lime from limestone: CaO + SiO2 → CaSiO3\text{CaO}\ +\ \text{SiO}_{2}\ \rightarrow \ \text{CaSiO}_{3}CaO + SiO2​ → CaSiO3​.
  • Basic gangue needs an acidic flux. Iron(II) oxide in copper smelting is removed with silica: FeO + SiO2 → FeSiO3\text{FeO}\ +\ \text{SiO}_{2}\ \rightarrow \ \text{FeSiO}_{3}FeO + SiO2​ → FeSiO3​.

The slag also shields the molten metal from the air.

Smelting and the matte

Heat a roasted sulphide ore of copper in a furnace with silica. The iron is slagged as FeSiO3\text{FeSiO}_{3}FeSiO3​. The copper stays as a molten mixture of Cu2S\text{Cu}_{2}\text{S}Cu2​S and FeS\text{FeS}FeS, called the copper matte. Copper(I) has a stronger pull for sulphur than iron does, so any copper oxide formed turns back into copper(I) sulphide. Course 3 follows the matte to the metal.

Self-reduction

Some sulphides can be roasted only part of the way. The oxide then reacts with the sulphide that is left, and the metal forms without any reducing agent. This is self-reduction, also called auto-reduction. For galena:

2PbS + 3O2 → 2PbO + 2SO22\text{PbS}\ +\ 3\text{O}_{2}\ \rightarrow \ 2\text{PbO}\ +\ 2\text{SO}_{2}2PbS + 3O2​ → 2PbO + 2SO2​, then PbS + 2PbO → 3Pb + SO2\text{PbS}\ +\ 2\text{PbO}\ \rightarrow \ 3\text{Pb}\ +\ \text{SO}_{2}PbS + 2PbO → 3Pb + SO2​

Copper is won the same way: 2Cu2O + Cu2S → 6Cu + SO22\text{Cu}_{2}\text{O}\ +\ \text{Cu}_{2}\text{S}\ \rightarrow \ 6\text{Cu}\ +\ \text{SO}_{2}2Cu2​O + Cu2​S → 6Cu + SO2​.

How much should be roasted? Each mole of lead sulphide left needs two moles of lead oxide. So two thirds of the galena is roasted and one third is left.

Practise with new numbers

Try it in Python

The program works out the zinc oxide, the sulphur dioxide and the air for roasting a batch of zinc blende.

Read it first. Predict the air needed if there were no excess. Then run it.

1. Change excess to 0. By what factor does the air change?

2. Change the program for galena, PbS\text{PbS}PbS (239) giving PbO\text{PbO}PbO (223). Which numbers change?

Common mistakes

  • Roasting a carbonate. A carbonate is calcined. Roasting is for sulphides and needs air.
  • Choosing a basic flux for a basic gangue. A flux must react with the gangue, so acid meets base.
  • Taking one carbon dioxide off dolomite. It loses two.
  • Thinking self-reduction needs carbon. The oxide and the sulphide reduce each other.

Remember these

  • Calcination: heat without much air, for carbonates and hydrated oxides; gives carbon dioxide or water.
  • Roasting: heat in air, for sulphides; gives the oxide and sulphur dioxide.
  • Flux plus gangue gives slag: CaSiO3\text{CaSiO}_{3}CaSiO3​ for iron, FeSiO3\text{FeSiO}_{3}FeSiO3​ for copper.
  • Self-reduction: PbS + 2PbO → 3Pb + SO2\text{PbS}\ +\ 2\text{PbO}\ \rightarrow \ 3\text{Pb}\ +\ \text{SO}_{2}PbS + 2PbO → 3Pb + SO2​ and Cu2S + 2Cu2O → 6Cu + SO2\text{Cu}_{2}\text{S}\ +\ 2\text{Cu}_{2}\text{O}\ \rightarrow \ 6\text{Cu}\ +\ \text{SO}_{2}Cu2​S + 2Cu2​O → 6Cu + SO2​.

References

  • NCERT Chemistry Part I for Class 12 (2007 edition), Unit 6, the section on extraction of crude metal from concentrated ore.
  • Greenwood and Earnshaw, Chemistry of the Elements, the chapters on germanium, tin and lead and on zinc, cadmium and mercury.

Check yourself

Try each one on your own first. If you are stuck, open a hint. Then check with Show the answer.

  1. Is zinc blende calcined or roasted? Write the equation.
  1. Why is silica added in the smelting of a copper ore that holds iron?
  1. What mass of carbon dioxide comes off when 250 kg of pure calamine, ZnCO3\text{ZnCO}_{3}ZnCO3​ (125.4 g/mol), is calcined?
  1. In the self-reduction of galena, why is only part of the ore roasted?

Enroll free in Ores and Their Concentration: Minerals, Flotation, Leaching and Roasting

Every lesson is open to read. Enrolling also lets you:

  • Mark lessons done and carry on where you stopped.
  • Take the tests of this lesson and its course.
  • Count the course towards the certificate for its chapter.
No payment. You can leave at any time.

Problems (4)

A 10.0 kg sample of calamine ore holds zinc carbonate, ZnCO₃, and silica only…Hard · High School (11–12) · by StemPy Lab
A smelter roasts 1.00 tonne of a zinc blende concentrate that holds 80.0 % ZnS, and the rest is…Advanced · High School (11–12) · by StemPy Lab
In a copper converter, 500 kg of iron(II) sulphide, FeS, in the matte is oxidised in a blast of…Hard · High School (11–12) · by StemPy Lab
That was the last lessonBack to the course: take the test
← Ores and Their Concentration: Minerals, Flotation, Leaching and Roasting
← Concentrating an ore: washing, magnets, froth and leachingNext →

Discussion (0)

Log in to join the discussion.

Loading…

1 Python program
4 questions to check yourself

This lesson is free to read. Enroll free to keep your place and take the tests.

Calcination, roasting, flux and slag
A small smelter treats 717 kg of pure galena, PbS…Advanced · High School (11–12) · by StemPy Lab

Question Sets (1)

Ores and Concentration: Check Your Understanding10 questions · by StemPy Lab

Notes (1)

Ores and Their Concentration: Quick RevisionNote · by StemPy Lab