  • Physics
  • Chemistry
  • Mathematics
  • Biology
  • Python Programming
  • Statistics & Data Science
  • Computer Science
  • Space Science and Astronomy
  • Classes
  • Groups

Practice

  • Problems
  • Quizzes
  • Mock Tests
  • Prepare for an Exam
  • Question Sets
  • Exams
  • Certificates
  • Python Labs
  • AI Practice Generator
  • Student-Created Tests

Community

  • Discussions
  • Resources
  • Notes
  • Glossary
  • Blog

Account

  • Log in
© 2026 senLearn. All rights reserved.HelpFor SchoolsAboutContactPrivacy PolicyTerms of UseRefund Policy
Electrolysis, Refining and the Extraction of Four Metals
  1. 1Electrochemical extraction: aluminium, displacement and chlorine
  2. 2Refining a crude metal
  3. 3Iron, copper and zinc from ore to metal, with uses and recycling
  1. Chemistry
  2. /Electrolysis, Refining and the Extraction of Four Metals
  3. /Refining a crude metal

Course 35.3·Lesson 2 of 3

Refining a crude metal

A metal from the furnace is never pure. Copper for wires must be more than 99.9 % copper, and silicon for chips must be purer still. How is that done? This lesson sets out the methods of refining and the property of the metal that each one uses.

about 25 min1 simulation1 practice question
Lesson 2 of 3Show all lessonsHide
Electrolysis, Refining and the Extraction of Four Metals
  1. 1Electrochemical extraction: aluminium, displacement and chlorine
  2. 2Refining a crude metal
  3. 3

Try the code and the simulations beside the lesson.

Why refine?

The crude metal carries other metals, carbon, sulphur and oxides. A little impurity changes a metal a lot. For example, a trace of arsenic makes copper conduct much worse. Each refining method uses a difference between the metal and its impurities.

Distillation

Metals with a low boiling point, such as zinc (1180 K) and mercury (630 K), are boiled off and condensed. The impurities stay behind.

Liquation

A metal with a low melting point, such as tin, is heated on a sloping hearth. The metal melts and flows down. The impurities that melt at a higher temperature stay on the hearth.

Poling

Molten blister copper still holds some copper(I) oxide. It is stirred with logs of green wood. The gases and hydrocarbons from the wood reduce the oxide to copper.

Electrolytic refining

The impure metal is the anode. A thin strip of pure metal is the cathode. The electrolyte is a solution of a salt of the metal. For copper, it is copper(II) sulphate acidified with sulphuric acid.

Electrolytic refining of copper. A tank holds an acidified solution of copper(II) sulphate. On the left a thick slab of impure copper is the anode, marked plus. On the right a thin sheet of pure copper is the cathode, marked minus. Copper(II) ions move from the anode to the cathode. Under the anode a layer of anode mud holds silver, gold and platinum.

At the anode: Cu → Cu2+ + 2e−\text{Cu}\ \rightarrow \ \text{Cu}^{2+}\ +\ 2\text{e}^{-}Cu → Cu2+ + 2e−. At the cathode: Cu2+ + 2e− → Cu\text{Cu}^{2+}\ +\ 2\text{e}^{-}\ \rightarrow \ \text{Cu}Cu2+ + 2e− → Cu.

So copper only moves from the anode to the cathode, and the cell voltage is small, about 0.2 to 0.4 V.

  • More reactive impurities, such as iron and zinc, also dissolve at the anode. They stay in the solution and are not plated, because their ions are harder to reduce than copper ions.
  • Less reactive impurities, such as silver, gold and platinum, do not dissolve. They fall to the bottom as the anode mud, which is worth more than the copper. Antimony, selenium and tellurium also collect there.

Zinc is refined in the same way, with zinc sulphate as the electrolyte.

Zone refining

This method gives metals of very high purity, as needed for semiconductors: silicon, germanium, boron, gallium and indium. It rests on one fact: impurities are more soluble in the melt than in the solid.

A ring heater melts a narrow zone of a bar and moves slowly along it. Pure metal freezes behind the zone. The impurities stay in the molten zone and are swept to one end, which is cut off. The pass is repeated many times.

The distribution coefficient kkk is the ratio of impurity in the freezing solid to that in the melt. After one pass, at a distance xxx along a bar, with a zone of length lll,

CC0=1−(1−k) e−kx/l\displaystyle \dfrac{C}{C_0} = 1 - (1 - k)\,e^{-kx/l}C0​C​=1−(1−k)e−kx/l

where C0C_0C0​ is the impurity before the pass.

A graph of the impurity left in a bar after one pass of a molten zone, as a fraction of the starting impurity, against the distance along the bar in zone lengths, from 0 to 20. Three curves for distribution coefficients of 0.1, 0.3 and 0.6. Each curve starts at its own coefficient at the start of the bar and rises toward 1. The curve for 0.1 starts lowest and rises most slowly.

Set k=0.2k = 0.2k=0.2. The start of the bar keeps only a fifth of its impurity after one pass. Then set k=0.6k = 0.6k=0.6. The cleaning is much weaker. Plants with a large kkk simply repeat the pass many times.

Vapour phase refining

The metal is turned into a volatile compound, which is collected and then broken down to give the pure metal.

The Mond process for nickel. Crude nickel is heated in a stream of carbon monoxide at 330 to 350 K. Volatile nickel tetracarbonyl forms, and the impurities stay solid.

Ni + 4CO → Ni(CO)4\text{Ni}\ +\ 4\text{CO}\ \rightarrow \ \text{Ni}(\text{CO})_{4}Ni + 4CO → Ni(CO)4​ at 330 to 350 K

The carbonyl vapour is heated to 450 to 470 K, where it breaks up into pure nickel and carbon monoxide, which is used again.

Ni(CO)4 → Ni + 4CO\text{Ni}(\text{CO})_{4}\ \rightarrow \ \text{Ni}\ +\ 4\text{CO}Ni(CO)4​ → Ni + 4CO at 450 to 470 K

The van Arkel method for zirconium and titanium. It removes oxygen and nitrogen, which spoil these metals. The crude metal is heated with iodine in an evacuated vessel. The volatile iodide forms:

Zr + 2I2 → ZrI4\text{Zr}\ +\ 2\text{I}_{2}\ \rightarrow \ \text{ZrI}_{4}Zr + 2I2​ → ZrI4​

The iodide vapour meets a tungsten filament heated electrically to about 1800 K. It breaks up, and pure metal is deposited on the filament.

ZrI4 → Zr + 2I2\text{ZrI}_{4}\ \rightarrow \ \text{Zr}\ +\ 2\text{I}_{2}ZrI4​ → Zr + 2I2​

Chromatography

A mixture is put on a column of an adsorbent, such as alumina. A liquid moves through the column. The parts of the mixture are held back to different extents, so they come out at different times. Column chromatography purifies elements that are available only in small amounts, and elements whose impurities are very like them in chemistry.

Practise with new numbers

Try it in Python

The program works out the copper plated in a refining cell in a day, the silver that collects in the anode mud, and the energy used.

Read it first. Predict how the energy per tonne compares with the aluminium cell. Then run it.

1. Change silver_share to 0.001. How much silver collects now?

2. Why is the voltage of this cell so much smaller than that of an aluminium cell?

Common mistakes

  • Putting the pure copper at the anode. The impure metal is the anode, and it dissolves.
  • Saying iron collects in the anode mud. Iron dissolves and stays in the solution. Only the less reactive metals fall as mud.
  • Mixing the Mond temperatures. Low temperature forms the carbonyl; higher temperature breaks it.
  • Thinking zone refining works because impurities are less soluble in the melt. They are more soluble in the melt.

Remember these

  • Distillation: Zn, Hg. Liquation: Sn. Poling: copper(I) oxide in copper.
  • Electrolytic: impure anode, pure cathode, salt solution; anode mud holds Ag, Au, Pt.
  • Zone refining: Si, Ge, Ga, B, In; impurities stay in the melt; C/C0=1−(1−k)e−kx/lC/C_0 = 1 - (1 - k)e^{-kx/l}C/C0​=1−(1−k)e−kx/l after one pass.
  • Mond: Ni, 330 to 350 K then 450 to 470 K. Van Arkel: Zr, Ti, iodide on a tungsten filament at 1800 K.

References

  • NCERT Chemistry Part I for Class 12 (2007 edition), Unit 6, the section on refining.
  • Greenwood and Earnshaw, Chemistry of the Elements, the chapters on nickel and on titanium, zirconium and hafnium.

Check yourself

Try each one on your own first. If you are stuck, open a hint. Then check with Show the answer.

  1. In the electrolytic refining of copper, where do silver and iron impurities end up?
  1. Which property of the impurities does zone refining use?
  1. Write the two steps of the Mond process with their temperatures.
  1. Why is tin refined by liquation?

Enroll free in Electrolysis, Refining and the Extraction of Four Metals

Every lesson is open to read. Enrolling also lets you:

  • Mark lessons done and carry on where you stopped.
  • Take the tests of this lesson and its course.
  • Count the course towards the certificate for its chapter.
No payment. You can leave at any time.

Problems (3)

A copper refinery tank runs at 25.0 kA for 24 hours with a current efficiency of 96 %…Hard · High School (11–12) · by StemPy Lab
A germanium bar is zone refined. For one impurity the distribution coefficient is k = 0.10: the…Advanced · High School (11–12) · by StemPy Lab
A refinery treats 500 g of crude nickel that is 95.0 % nickel by the Mond process, and all the…Hard · High School (11–12) · by StemPy Lab
Next: lesson 3Iron, copper and zinc from ore to metal, with uses and recycling
← Electrolysis, Refining and the Extraction of Four Metals
← Electrochemical extraction: aluminium, displacement and chlorineIron, copper and zinc from ore to metal, with uses and recycling →

Discussion (0)

Log in to join the discussion.

Loading…

1 Python program
4 questions to check yourself

This lesson is free to read. Enroll free to keep your place and take the tests.

Iron, copper and zinc from ore to metal, with uses and recycling