HelpContactFor teachers and institutes
>_StemPy Lab
Mock TestsClasses

>_StemPy Lab

Learn. Solve. Code the solutions. Test yourself.

Live examsFree mock exams, timed and rankedEveryone starts together, and your score and rank come the moment it ends.See the exams →
Live examsInternational live exams are comingTell us which exam you want first. Timed practice papers are open now.See what is coming →

Learn

  • Physics
  • Chemistry
  • Mathematics
  • Biology
  • Python Programming
  • Statistics & Data Science
  • Computer Science
  • Space Science and Astronomy
  • Classes
  • Groups

Practice

  • Problems
  • Quizzes
  • Mock Tests
  • Prepare for an Exam
  • Question Sets
  • Exams
  • Certificates
  • Python Labs
  • AI Practice Generator
  • Student-Created Tests

Community

  • Discussions
  • Resources
  • Notes
  • Glossary
  • Blog

Account

  • Log in
© 2026 senLearn. All rights reserved.HelpFor SchoolsAboutContactPrivacy PolicyTerms of UseRefund Policy
  1. Notes
  2. /Ores and Their Concentration: Quick Revision
Chemistry

Ores and Their Concentration: Quick Revision

A brief note on ores and their concentration. Minerals and ores, the ores of aluminium, iron, copper and zinc, the methods of concentration, leaching, calcination, roasting and slag, with a worked example, practice, a program and questions.

StemPy LabWritten by StemPy Lab
Log in to save

A brief note on Ores and Their Concentration. Read it before a test. Try each question at the end before you open its answer.

Ores

  • A mineral is a natural compound. An ore gives the metal at a profit. Gangue is the unwanted rock.
  • Aluminium: bauxite AlOx(OH)3-2x\text{AlOx}(\text{OH})_{3}\text{-}_{2}\text{x}AlOx(OH)3​-2​x. Iron: haematite Fe2O3\text{Fe}_{2}\text{O}_{3}Fe2​O3​, magnetite Fe3O4\text{Fe}_{3}\text{O}_{4}Fe3​O4​, siderite FeCO3\text{FeCO}_{3}FeCO3​.
  • Copper: copper pyrites CuFeS2\text{CuFeS}_{2}CuFeS2​, malachite CuCO3⋅Cu(OH)2\text{CuCO}_{3}\cdot \text{Cu}(\text{OH})_{2}CuCO3​⋅Cu(OH)2​, cuprite Cu2O\text{Cu}_{2}\text{O}Cu2​O, copper glance Cu2S\text{Cu}_{2}\text{S}Cu2​S.
  • Zinc: zinc blende ZnS\text{ZnS}ZnS, calamine ZnCO3\text{ZnCO}_{3}ZnCO3​, zincite ZnO\text{ZnO}ZnO.

Concentration

  • Hydraulic washing: the denser ore stays, the light gangue is washed away.
  • Magnetic separation: magnetite, chromite, wolframite are attracted.
  • Froth flotation: for sulphides. Collector (pine oil, xanthate), froth stabiliser (cresol, aniline), depressant (NaCN for ZnS).
  • Bayer process: Al2O3 + 2NaOH + 3H2O → 2Na[Al(OH)4]\text{Al}_{2}\text{O}_{3}\ +\ 2\text{NaOH}\ +\ 3\text{H}_{2}\text{O}\ \rightarrow \ 2\text{Na}[\text{Al}(\text{OH})_{4}]Al2​O3​ + 2NaOH + 3H2​O → 2Na[Al(OH)4​]. Red mud Fe2O3\text{Fe}_{2}\text{O}_{3}Fe2​O3​ is left. Carbon dioxide and seeding give hydrated alumina; heating at 1470 K gives Al2O3\text{Al}_{2}\text{O}_{3}Al2​O3​.
  • Cyanide process: gold and silver dissolve as [M(CN)2]−[\text{M}(\text{CN})_{2}]^{-}[M(CN)2​]− in air. Zinc displaces them.

Calcination and roasting

  • Calcination, little or no air: ZnCO3 → ZnO + CO2\text{ZnCO}_{3}\ \rightarrow \ \text{ZnO}\ +\ \text{CO}_{2}ZnCO3​ → ZnO + CO2​, Fe2O3⋅xH2O → Fe2O3 + xH2O\text{Fe}_{2}\text{O}_{3}\cdot \text{xH}_{2}\text{O}\ \rightarrow \ \text{Fe}_{2}\text{O}_{3}\ +\ \text{xH}_{2}\text{O}Fe2​O3​⋅xH2​O → Fe2​O3​ + xH2​O.
  • Roasting, in air: 2ZnS + 3O2 → 2ZnO + 2SO22\text{ZnS}\ +\ 3\text{O}_{2}\ \rightarrow \ 2\text{ZnO}\ +\ 2\text{SO}_{2}2ZnS + 3O2​ → 2ZnO + 2SO2​.
  • Flux and slag: CaO + SiO2 → CaSiO3\text{CaO}\ +\ \text{SiO}_{2}\ \rightarrow \ \text{CaSiO}_{3}CaO + SiO2​ → CaSiO3​ for iron; FeO + SiO2 → FeSiO3\text{FeO}\ +\ \text{SiO}_{2}\ \rightarrow \ \text{FeSiO}_{3}FeO + SiO2​ → FeSiO3​ for copper.
  • Self-reduction: PbS + 2PbO → 3Pb + SO2\text{PbS}\ +\ 2\text{PbO}\ \rightarrow \ 3\text{Pb}\ +\ \text{SO}_{2}PbS + 2PbO → 3Pb + SO2​.

A worked example

How much iron is in 3.00 t of an ore with 40.0 % haematite?

  1. Haematite. 3000 kg×0.400=1200 kg3000\ \text{kg} \times 0.400 = 1200\ \text{kg}3000 kg×0.400=1200 kg.
  2. Iron. 1200 kg×112160=840 kg1200\ \text{kg} \times \dfrac{112}{160} = 840\ \text{kg}1200 kg×160112​=840 kg.

Practice with new numbers

A program to try

The program works out the metal in a tonne of ore for four minerals.

Run it. Which mineral gives the least metal?

1. Change mineral_percent to 90 and run it again.

Mistakes to avoid

  • Froth flotation for an oxide ore. It is for sulphides.
  • Calling iron oxide soluble in the Bayer process. It is the red mud.
  • Roasting a carbonate. Carbonates are calcined.

Check yourself

  1. Which reagent depresses zinc blende in flotation?
  1. What is the red mud of the Bayer process?
  1. Why is air needed in the cyanide process?
  1. Which flux removes silica from an iron ore?
← All Notes
← Sodium and Calcium Compounds: Quick RevisionThermodynamics of Extraction: Quick Revision →
More onGeneral Principles and Processes of Isolation of Elements

Discussion (0)

Log in to join the discussion.

Loading…

On this page

  1. Ores
  2. Concentration
  3. Calcination and roasting
  4. A worked example
  5. Practice with new numbers
  6. A program to try
  7. Mistakes to avoid
  8. Check yourself

Goes with the lesson

  1. Calcination, roasting, flux and slagOres and Their Concentration: Minerals, Flotation, Leaching and Roasting

More notes on this topic

  1. Electrolysis, Refining and Extraction: Quick Revision
  2. Thermodynamics of Extraction: Quick Revision
All notes on this topic →