A brief note on Electrolysis, Refining and Extraction . Read it before a test. Try each question at the end before you open its answer.
Δ G ∘ = − n F E ∘ \Delta G^\circ = -nFE^\circ Δ G ∘ = − n F E ∘ . Mass: m = η I t M / ( n F ) m = \eta ItM/(nF) m = η I tM / ( n F ) . Hall-Heroult: alumina in molten cryolite near 1220 K; carbon lining is the cathode, graphite blocks the anodes. Cathode Al 3 + + 3 e − → Al \text{Al}^{3+}\ +\ 3\text{e}^{-}\ \rightarrow \ \text{Al} Al 3 + + 3 e − → Al ; anode carbon burns to CO and CO 2 \text{CO}_{2} CO 2 ; overall 2 Al 2 O 3 + 3 C → 4 Al + 3 CO 2 2\text{Al}_{2}\text{O}_{3}\ +\ 3\text{C}\ \rightarrow \ 4\text{Al}\ +\ 3\text{CO}_{2} 2 Al 2 O 3 + 3 C → 4 Al + 3 CO 2 . Displacement: Cu 2 + + Fe → Cu + Fe 2 + \text{Cu}^{2+}\ +\ \text{Fe}\ \rightarrow \ \text{Cu}\ +\ \text{Fe}^{2+} Cu 2 + + Fe → Cu + Fe 2 + , E ∘ = 0.78 V E^\circ = 0.78\ \text{V} E ∘ = 0.78 V . Chlorine: oxidation of chloride in brine, E ∘ ≈ − 2.2 V E^\circ \approx -2.2\ \text{V} E ∘ ≈ − 2.2 V . Refining Distillation: Zn, Hg. Liquation: Sn. Poling: copper. Electrolytic: impure anode, pure cathode; Ag, Au, Pt in the anode mud. Zone refining: Si, Ge, Ga, B, In; impurities stay in the melt. Mond: Ni + 4 CO → Ni ( CO ) 4 \text{Ni}\ +\ 4\text{CO}\ \rightarrow \ \text{Ni}(\text{CO})_{4} Ni + 4 CO → Ni ( CO ) 4 at 330 to 350 K; breaks up at 450 to 470 K. Van Arkel: Zr + 2 I 2 → ZrI 4 \text{Zr}\ +\ 2\text{I}_{2}\ \rightarrow \ \text{ZrI}_{4} Zr + 2 I 2 → ZrI 4 , broken up on tungsten at about 1800 K. Chromatography: for small amounts and look-alike impurities. Iron: blast furnace; CO at the top, C and CO in the middle, slag CaSiO 3 \text{CaSiO}_{3} CaSiO 3 . Pig iron about 4 % C; wrought iron purest. Copper: flotation, roasting, matte, converter, blister copper, electrolysis. Zinc: roast, then coke near 1673 K or electrolysis of zinc sulphate. Recycling aluminium needs about 5 % of the energy. A worked example What mass of copper does a refining cell plate in 10.0 hours at 2.00 kA, all the current used?
Charge. 2000 A × 36 000 s = 7.20 × 10 7 C 2000\ \text{A} \times 36\,000\ \text{s} = 7.20 \times 10^7\ \text{C} 2000 A × 36 000 s = 7.20 × 1 0 7 C . Copper. 7.20 × 10 7 2 × 96 485 × 63.5 g/mol = 23.7 kg \dfrac{7.20 \times 10^7}{2 \times 96\,485} \times 63.5\ \text{g/mol} = 23.7\ \text{kg} 2 × 96 485 7.20 × 1 0 7 × 63.5 g/mol = 23.7 kg . Practice with new numbers
A program to try The program follows an aluminium cell for one day.
Run it. How much aluminium does the cell make in a day?
1. Change current to 300_000 and run it again.
Mistakes to avoid Aluminium takes three electrons, copper and zinc two. Iron does not fall into the anode mud. It dissolves. Mond: form low, break high. Check yourself What are the cathode and anode of a Hall-Heroult cell? Stuck? Show a hint Show the answerWhich metals collect in the anode mud of a copper refinery? Stuck? Show a hint Show the answerWhich zone of the blast furnace reduces haematite, and with what? Stuck? Show a hint Show the answerWhat is blister copper? Stuck? Show a hint Show the answer